APA honors eight departments of transportation for excellent asphalt roads

By

Eight departments of transportation were named winners of the 2017 Perpetual Pavement Award by Asphalt Pavement Alliance (APA). The award celebrates long-life asphalt pavements that reflect the characteristics of a perpetual pavement design.

The award is presented to state transportation departments and local agency road owners for well-performing asphalt pavements that are at least 35 years old with proven high-quality structural design. To earn the award, the pavement must not have suffered a structural failure, and it should have an average interval between resurfacings of no less than 13 years. The pavement must demonstrate the characteristics expected from a long-life, perpetual pavement design: excellence in design, quality in construction and value for the taxpayers.

The 2017 winners are:

Alabama Department of Transportation, North Region for a 4-mile section of four-lane divided highway on U.S. Highway 72/State Route 2 in Jackson County, from County Road 11 to SR 79. This is the ninth APA Perpetual Pavement Award for ALDOT.

Arkansas Department of Transportation for a 2-mile stretch of two-lane Arkansas Highway 24/Section 6 in Ouachita County. This is the eighth APA Perpetual Pavement Award for ARDOT.

Florida Department of Transportation for a 4.265-mile section of rural two-lane arterial roadway on Florida State Road 50 in Sumter County. This is the eighth APA Perpetual Pavement Award for FDOT.

Minnesota Department of Transportation for a 4.75 section of two-lane road on Minnesota State Highway 89 in Beltrami County. Sixteen MnDOT pavements have earned an APA Perpetual Pavement Award, more than any other state.

Pennsylvania Department of Transportation, Engineering District 3-0 for a 4.5 section of two-lane road on State Route 3010 in Columbia County. PennDOT has earned seven APA Perpetual Pavement Awards.

South Carolina Department of Transportation for a 9-mile section of four-lane divided highway on Interstate 95 in Jasper County. SCDOT has earned seven APA Perpetual Pavement Awards.

Tennessee Department of Transportation for a 3.7-mile stretch of two-lane highway on State Route 88 in Lauderdale County. This is the 13th APA Perpetual Pavement Award earned by TDOT.

Washington State Department of Transportation for a 4.42-mile section of four-lane divided highway on State Route 16 in Pierce and Kitsap counties. This is the fourth APA Perpetual Pavement Award earned by WSDOT.

“One of the keys to sustainability is long life,” said Amy Miller, P.E., national director of the Asphalt Pavement Alliance. “These Perpetual Pavement Award-winning roads demonstrate how asphalt roads can be engineered to last indefinitely with only routine maintenance and periodic surface renewal.”

Engineers at the National Center for Asphalt Technology (NCAT) at Auburn University, evaluated the nominations and validated the results for the eight 2017 Perpetual Pavement Award winners.

Winning agencies are honored by their local state asphalt pavement association and are presented with an engraved crystal obelisk. The names of the winning agencies and projects are added to a plaque on permanent display at the NCAT Research Center at Auburn University. Since the Perpetual Pavement Award was first presented in 2001, 126 pavements in 30 U.S. states and one Canadian province have been honored with the award.

The Asphalt Pavement Alliance is a partnership of the Asphalt Institute (AI), National Asphalt Pavement Association (NAPA) and the State Asphalt Pavement Associations. The Asphalt Pavement Alliance’s mission is to establish asphalt as the preferred choice for quality, performance and the environment.

 

Advertisement
Advertisement HollyFrontier
Advertisement Asphalt Day
Advertisement J-Band
Advertisement HollyFrontier